Immediately following impression forging, the part being forged shall be normalized for 1 hr at 1,650 °F (899 °C) then air cooled.
Loading…
AISC 358-22, Prequalified Connections for Special and Intermediate Steel Moment Frames for Seismic Applications
Last Updated 29 Oct 2026
Hover any section to copy its link or text, ask Copilot about it, or bookmark it.
Immediately following impression forging, the part being forged shall be normalized for 1 hr at 1,650 °F (899 °C) then air cooled.